Tevo Tornado - quick solution to first layer adhesion and avoid warping
1) measure around 300ml of water
2) add sugar to it until it cant dissolve anymore (saturation)
3) apply on the print bed
4) heat up to 60degC for PLA
5) use a brim for print model in slicer
6) start print when dry
7) adjust z-offset accordingly as extruder lays the first later
8) tape down the brim after it is printed
...Read more!...